Instruction of coating
1. Make sure clean the surface of media, and there is no oil and dusk on it.
2. Soak the clean media in the container filled with coating or spray coating evenly onto the surface of media with spray bottle. After even spray, hang it on the shelf to dry, which generally takes 2 hours. After no water dripping,
Put the media on the 150-degree oven to bake, and set the time 55 minutes. When time is up, take it out and use.
NEXT PAGE:FUZHOU OBOOC TECHNOLOGY CO.,LTD
PREV PAGE:The reason why printer head is clogged
- Why do you have to dye your fingers purple before voting?
- A variety of products of Obooc appeared at the Canton Fair
- Obooc appeared at the 136th Canton Fair and was well received by customers around the world
- One stroke to fix it ▏ Have you used the powerful paint pen?
- How to erase stubborn whiteboard pen marks?
- See the fleeting time, come and get some beautiful gold powder ink classic combinations
- What is the difference between textile direct-jet ink and thermal transfer ink?
- Obooc carton ink has stable quality and refuses to waste cardboard!
- Tel: +86 591 83303835
- Fax: +86 591 88201182
- Phone: Wechat/Whatsapp +86 13313769052
- Email: sales04@obooc.com
- Website: www.indelibleink.com.cn